The effect of a pre (before) and post (after) heating welding treatment on the microstructure and mechanical properties of the scrap blades made of cast INC738LC superalloy is the main goal of the present investigation. The filler used in TIG welding was a INC 625 solution hardened superalloy as the proposed solution for hot cracking of the INC738LC cast superalloy in literature. The ... https://www.roneverhart.com/Apple-Watch-Ultra-2-GPS-Cellular-49mm-Titanium-Case-with-Blue-Black-Trail-Loop-S-M-MRF53LL-A/